Li-La-Zr-O固态电解质包覆对富锂锰基层状正极材料性能影响
首发时间:2017-05-22
摘要:采用溶胶-凝胶法在富锂锰基正极材料Li1.188Ni0.198Co0.087Mn0.553O2 (LMO)表面成功包覆上了Li-La-Zr-O(LLZO)固态电解质层。运用SEM、TEM、XRD、ICP-AES、EIS等技术对LLZO包覆前后的材料进行了表征。恒流充放电测试得到2 wt% LLZO包覆的富锂材料(LMO@LLZO)在1C下循环450圈后人具有193mAh/g的容量,循环保持率为84.8%;而在相同条件下,未包覆的材料仅剩125.4 mAh/g容量,循环保持率为54.1%。这主要是由于Li-La-Zr-O包覆层提高了富锂材料表面的稳定性,有效的抑制了副反应的发生。另外,2 wt% LLZO的包覆层还能通过降低传荷阻抗来提高材料的倍率性能。
关键词: 锂离子电池 富锂锰基层状正极材料 固态电解质包覆 电化学性能。
For information in English, please click here
Superior electrochemical performance of Li-rich layered cathode material by coating Li-La-Zr-O solid electrolyte
Abstract:A Li-rich Mn-based layered oxide Li1.188Ni0.198Co0.087Mn0.553O2 (LMO) material was successfully coated with Li-La-Zr-O solid electrolyte (LLZO) by sol-gel process. Both LLZO-coated LMO and pristine materials were characterized by x-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), inductively coupled plasma-atomic emission spectrometry (ICP-AES) and electrochemical impedance spectroscopy (EIS) to explore the effect of LLZO coating layer. Galvanostatic charge-discharge tests indicate that after 450 cycles at 1 C, the 2 wt% LLZO-coated LMO material (LMO@LLZO) exhibits a significant cycle stability of 193 mAh g-1 capacity with a capacity retention of 84.8 % compared to the LMO material of 125.4 mAh g-1 capacity with a capacity retention of 54.1 %. This is because the Li-La-Zr-O coating layer improve the surface stability and suppressed side reactions. In addition, the 2 wt% LLZO coating layer could also improve the rate performance of the electrode by obviously reducing interfacial charge-transfer resistance.)
Keywords: lithium-ion battery Li-rich layered oxide solid electrolyte coating electrochemical performance
论文图表:
引用

No.4734885119309214****
同行评议
共计0人参与
勘误表
Li-La-Zr-O固态电解质包覆对富锂锰基层状正极材料性能影响
评论
全部评论